Boiler Plate
Boiler sheets are the type of steel plate used in the manufacture of boilers, as you can understand from the name. They are generally used in the internal structures of boilers. Boiler steels that are suitable for use under high temperature and pressure are used in the manufacture of boiler sheets, pressure vessels and boilers due to their excellent forming and weldability properties. Continuous operation up to approximately 450 °C and wall temperatures up to 450 °C possible. Boiler sheets are steel resistant to pressure. Commercial grade steels start with the S quality nomenclature, such as S235JR, and boiler sheets are P group steels. P235GH quality .P265GH quality, P355GH quality, 16M03 Quality P295GH Quality, P355NH Quality, P355NL1 quality.
Only Erdemir produces P235GH Quality Boiler Sheets in Turkey. P235GH Quality steel sheets are 6335 quality, corresponding to Erdemir quality.
Usage areas
-In the manufacture of transport vehicles (ships, trains, trucks, buses, bicycles)
-In the energy sector; in energy transmission lines, wind power generation equipment, power plant construction, solar energy utilization equipment
-In the agricultural sector; in the construction of pipes used in agricultural machinery, in controlling the great power of water, in the construction of canals, tunnels, dams, bridges, ports
-Storage systems, silo construction, container manufacturing
-In hot and pressurized environments, in the manufacture of heat exchangers, in the manufacture of steam boilers
– It is used successfully in the construction industry in the construction of carrier columns, concrete transport, mixing, molding equipment, in the construction of steel buildings.
Sheet Grades
Chemical analysis of P235GH (6335) quality sheets
Unalloyed Boiler Steels Suitable for Use Under High Temperature and Pressure Standard : EN 10028-2:2017
Chemical Composition (%)
|
|
Standard Equivalent
|
ERDEMİR
Quality No
|
C
|
Si
max.
|
Mn
|
P max.
|
S max.
|
Al
min.
|
N(3)
max.
|
Cr(1) max.
|
Cu(1) max.
|
Mo(1)
max.
|
Nb
max.
|
Ni(1)
max.
|
Ti
max.
|
V max.
|
Standard
|
Quality
|
EN 10028-2
|
P235GH
|
6335(2)
|
0.16 max.
|
0.35
|
0.60-1.20
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.020
|
0.30
|
0.03
|
0.02
|
EN 10028-2
|
P265GH
|
6341(2)
|
0.20 max.
|
0.40
|
0.80-1.40
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.020
|
0.30
|
0.03
|
0.02
|
EN 10028-2
|
P295GH
|
63472
|
0.08 – 0.20
|
0.40
|
0.90-1.50
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.020
|
0.02
|
0.03
|
0.02
|
EN 10028-2
|
P355GH
|
6352
|
0.10 – 0.22
|
0.60
|
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.040
|
0.30
|
0.03
|
|
Descriptions
1) Cr + Cu + Mo + Ni sum max. It should be 0.70%.
2) For thicknesses less than 6 mm, minimum Mn amounts can be reduced by 0.20%.
Al / N > 2 ratio is applied.
Mechanical Properties
|
|
|
Standard Equivalent
|
ERDEMİR
Quality No
|
Re N/mm2 (kg/mm2)
|
Rm(1) N/mm2 (kg/mm2)
|
A5 (%) min.
|
Darbe(3)(4)
(Enine)
|
Rp0.2(1)(2)
N/mm2 (kg/mm2) Sıcaklık= 300°C
|
Sıc.
°C
|
KVc min.
J
|
d<16 min.
|
16<d<40 min.
|
40<d<50 min.
|
d<16
min.
|
16<d<40 min.
|
40<d<50 min.
|
Standard
|
Quality
|
EN 10028-2
|
P235GH
|
6335
|
235
( 24.0 )
|
225
( 22.9 )
|
215 ( 21.9 )
|
360 – 480 ( 36.7 – 49.0 )
|
24
|
-20
|
27
|
153 (15.6)
|
147 (15.0)
|
140 (14.3)
|
EN 10028-2
|
P265GH
|
6341
|
265
( 27.0 )
|
255 ( 26.0 )
|
245 ( 25.0 )
|
410 – 530
( 41.8 – 54.1 )
|
22
|
-20
|
27
|
173 (17.6)
|
166
(16.9)
|
160 (16.3)
|
EN 10028-2
|
P295GH
|
6347
|
295
( 30.1 )
|
290
( 29.6 )
|
285
( 29.1 )
|
460 – 580
( 46.9 – 59.2 )
|
21
|
-20
|
27
|
192 (19.6)
|
189
(19.3)
|
186 (19.0)
|
EN 10028-2
|
P355GH
|
6352
|
355 ( 36.2 )
|
345
( 35.2 )
|
335 ( 34.2 )
|
510 – 650 ( 52.0 – 66.3 )
|
20
|
-20
|
27
|
232 (23.7)
|
225
(22.9)
|
219 (22.3)
|
|
Descriptions
- Tensile test values are applied to ‘transverse’ test specimens,
Hot tensile test Optional.
- Impact test is not performed for products with a thickness of less than 6 mm.
- A minimum impact energy value of 40 J may be requested, subject to agreement.
Chemical analysis of P265GH (6341) quality boiler sheets
Unalloyed Boiler Steels Suitable for Use Under High Temperature and Pressure
Standard : EN 10028-2:2017
Chemical Composition (%)
|
|
Standard Equivalent
|
ERDEMİR
Quality No
|
C
|
Si
max.
|
Mn
|
P max.
|
S max.
|
Al
min.
|
N(3)
max.
|
Cr(1) max.
|
Cu(1) max.
|
Mo(1)
max.
|
Nb
max.
|
Ni(1)
max.
|
Ti
max.
|
V max.
|
Standard
|
Quality
|
EN 10028-2
|
P235GH
|
6335(2)
|
0.16 max.
|
0.35
|
0.60-1.20
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.020
|
0.30
|
0.03
|
0.02
|
EN 10028-2
|
P265GH
|
6341(2)
|
0.20 max.
|
0.40
|
0.80-1.40
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.020
|
0.30
|
0.03
|
0.02
|
EN 10028-2
|
P295GH
|
63472
|
0.08 – 0.20
|
0.40
|
0.90-1.50
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.020
|
0.30
|
0.03
|
0.02
|
EN 10028-2
|
P355GH
|
6352
|
0.10 – 0.22
|
0.60
|
1.10-1.70
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.040
|
0.30
|
0.03
|
0.02
|
ERDEMIR quality of P265GH quality pressure resistant sheets is 6341.
Descriptions
- Cr + Cu + Mo + Ni sum max. It should be 0.70%.
- For thicknesses less than 6 mm, the minimum Mn amounts can be reduced by 0.20%. Al / N > 2 ratio is applied. It starts from mm.
Mechanical Properties
|
|
Standard Equivalent
|
ERDEMİR
Quality No
|
Re N/mm2 (kg/mm2)
|
Rm(1) N/mm2 (kg/mm2)
|
A5 (%) min.
|
Darbe(3)(4)
(Enine)
|
Rp0.2(1)(2)
N/mm2 (kg/mm2) Sıcaklık= 300°C
|
Sıc.
°C
|
KVc min.
J
|
d<16 min.
|
16<d<40 min.
|
40<d<50 min.
|
d<16
min.
|
16<d<40 min.
|
40<d<50 min.
|
Standard
|
Quality
|
EN 10028-2
|
P235GH
|
6335
|
235
( 24.0 )
|
225
( 22.9 )
|
215 ( 21.9 )
|
360 – 480 ( 36.7 – 49.0 )
|
24
|
-20
|
27
|
153 (15.6)
|
147 (15.0)
|
140 (14.3)
|
EN 10028-2
|
P265GH
|
6341
|
265
( 27.0 )
|
255 ( 26.0 )
|
245 ( 25.0 )
|
410 – 530
( 41.8 – 54.1 )
|
22
|
-20
|
27
|
173 (17.6)
|
166
(16.9)
|
160 (16.3)
|
EN 10028-2
|
P295GH
|
6347
|
295
( 30.1 )
|
290
( 29.6 )
|
285
( 29.1 )
|
460 – 580
( 46.9 – 59.2 )
|
21
|
-20
|
27
|
192 (19.6)
|
189
(19.3)
|
186 (19.0)
|
EN 10028-2
|
P355GH
|
6352
|
355 ( 36.2 )
|
345
( 35.2 )
|
335 ( 34.2 )
|
510 – 650 ( 52.0 – 66.3 )
|
20
|
-20
|
27
|
232 (23.7)
|
225
(22.9)
|
219 (22.3)
|
Descriptions
- Tensile test values are applied to ‘transverse’ test specimens,
- Hot tensile test Optional.
- Impact test is not performed for products with a thickness of less than 6 mm.
- A minimum impact energy value of 40 J may be requested, subject to agreement.
ERDEMIR quality of P265GH quality pressure resistant sheets is 6341. The production range of Erdemir 6341 quality boiler sheets starts from 4mm.
Chemical Composition (%)
|
|
Standard Equivalent
|
ERDEMİR
Quality No
|
C
|
Si
max.
|
Mn
|
P max.
|
S max.
|
Al
min.
|
N(3)
max.
|
Cr(1) max.
|
Cu(1) max.
|
Mo(1)
max.
|
Nb
max.
|
Ni(1)
max.
|
Ti
max.
|
V max.
|
Standard
|
Quality
|
EN 10028-2
|
P235GH
|
6335(2)
|
0.16 max.
|
0.35
|
0.60-1.20
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.020
|
0.30
|
0.03
|
0.02
|
EN 10028-2
|
P265GH
|
6341(2)
|
0.20 max.
|
0.40
|
0.80-1.40
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.020
|
0.30
|
0.03
|
0.02
|
EN 10028-2
|
P295GH
|
63472
|
0.08 – 0.20
|
0.40
|
0.90-1.50
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.020
|
0.30
|
0.03
|
0.02
|
EN 10028-2
|
P355GH
|
6352
|
0.10 – 0.22
|
0.60
|
1.10-1.70
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.040
|
0.30
|
0.03
|
0.02
|
ERDEMIR quality of P265GH quality pressure resistant sheets is 6341. The production range of Erdemir 6341 quality boiler sheets starts from 4mm.
Descriptions
- Cr + Cu + Mo + Ni sum max. It should be 0.70%.
- For thicknesses less than 6 mm, the minimum Mn amounts can be reduced by 0.20%. Al / N > 2 ratio is applied.
Mechanical Properties
|
|
Standard Equivalent
|
ERDEMİR
Quality No
|
Re N/mm2 (kg/mm2)
|
Rm(1) N/mm2 (kg/mm2)
|
A5 (%) min.
|
Darbe(3)(4)
(Transverse)
|
Rp0.2(1)(2)
N/mm2 (kg/mm2) Heat= 300°C
|
Sıc.
°C
|
KVc min.
J
|
d<16 min.
|
16<d<40 min.
|
40<d<50 min.
|
d<16
min.
|
16<d<40 min.
|
40<d<50 min.
|
Standard
|
Quality
|
EN 10028-2
|
P235GH
|
6335
|
235
( 24.0 )
|
225
( 22.9 )
|
215 ( 21.9 )
|
360 – 480 ( 36.7 – 49.0 )
|
24
|
-20
|
27
|
153 (15.6)
|
147 (15.0)
|
140 (14.3)
|
EN 10028-2
|
P265GH
|
6341
|
265
( 27.0 )
|
255 ( 26.0 )
|
245 ( 25.0 )
|
410 – 530
( 41.8 – 54.1 )
|
22
|
-20
|
27
|
173 (17.6)
|
166
(16.9)
|
160 (16.3)
|
EN 10028-2
|
P295GH
|
6347
|
295
( 30.1 )
|
290
( 29.6 )
|
285
( 29.1 )
|
460 – 580
( 46.9 – 59.2 )
|
21
|
-20
|
27
|
192 (19.6)
|
189
(19.3)
|
186 (19.0)
|
EN 10028-2
|
P355GH
|
6352
|
355 ( 36.2 )
|
345
( 35.2 )
|
335 ( 34.2 )
|
510 – 650 ( 52.0 – 66.3 )
|
20
|
-20
|
27
|
232 (23.7)
|
225
(22.9)
|
219 (22.3)
|
Chemical Composition (%)
|
|
Standard Equivalent
|
ERDEMİR
Quality No
|
C
|
Si
max.
|
Mn
|
P max.
|
S max.
|
Al
min.
|
N(3)
max.
|
Cr(1) max.
|
Cu(1) max.
|
Mo(1)
max.
|
Nb
max.
|
Ni(1)
max.
|
Ti
max.
|
V max.
|
Standard
|
Quality
|
EN 10028-2
|
P235GH
|
6335(2)
|
0.16 max.
|
0.35
|
0.60-1.20
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.020
|
0.30
|
0.03
|
0.02
|
EN 10028-2
|
P265GH
|
6341(2)
|
0.20 max.
|
0.40
|
0.80-1.40
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.020
|
0.30
|
0.03
|
0.02
|
EN 10028-2
|
P295GH
|
63472
|
0.08 – 0.20
|
0.40
|
0.90-1.50
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.020
|
0.30
|
0.03
|
0.02
|
EN 10028-2
|
P355GH
|
6352
|
0.10 – 0.22
|
0.60
|
1.10-1.70
|
0.025
|
0.010
|
0.020
|
0.012
|
0.30
|
0.30
|
0.08
|
0.040
|
0.30
|
0.03
|
0.02
|
ERDEMIR quality of P265GH quality pressure resistant sheets is 6341. The production range of Erdemir 6341 quality boiler sheets starts from 4mm.
Descriptions
- Cr + Cu + Mo + Ni sum max. It should be 0.70%.
- For thicknesses less than 6 mm, the minimum Mn amounts can be reduced by 0.20%.
Al / N > 2 ratio is applied.
ERDEMIR quality equivalent of P355GH quality steels is 6352 Quality. Erdemir 6352 quality boiler sheets have a very high resistance to pressure. In addition, there are steels used in the production of pressure resistant pipes produced by Erdemir.
Mechanical Properties
|
|
Standard Equivalent
|
ERDEMİR
Quality No
|
Re N/mm2 (kg/mm2)
|
Rm(1) N/mm2 (kg/mm2)
|
A5 (%) min.
|
Darbe(3)(4)
(Enine)
|
Rp0.2(1)(2)
N/mm2 (kg/mm2) Sıcaklık= 300°C
|
Sıc.
°C
|
KVc min.
J
|
d<16 min.
|
16<d<40 min.
|
40<d<50 min.
|
d<16
min.
|
16<d<40 min.
|
40<d<50 min.
|
Standard
|
Quality
|
EN 10028-2
|
P235GH
|
6335
|
235
( 24.0 )
|
225
( 22.9 )
|
215 ( 21.9 )
|
360 – 480 ( 36.7 – 49.0 )
|
24
|
-20
|
27
|
153 (15.6)
|
147 (15.0)
|
140 (14.3)
|
EN 10028-2
|
P265GH
|
6341
|
265
( 27.0 )
|
255 ( 26.0 )
|
245 ( 25.0 )
|
410 – 530
( 41.8 – 54.1 )
|
22
|
-20
|
27
|
173 (17.6)
|
166
(16.9)
|
160 (16.3)
|
EN 10028-2
|
P295GH
|
6347
|
295
( 30.1 )
|
290
( 29.6 )
|
285
( 29.1 )
|
460 – 580
( 46.9 – 59.2 )
|
21
|
-20
|
27
|
192 (19.6)
|
189
(19.3)
|
186 (19.0)
|
EN 10028-2
|
P355GH
|
6352
|
355 ( 36.2 )
|
345
( 35.2 )
|
335 ( 34.2 )
|
510 – 650 ( 52.0 – 66.3 )
|
20
|
-20
|
27
|
232 (23.7)
|
225
(22.9)
|
219 (22.3)
|
|
Descriptions
- Tensile test values are applied to ‘transverse’ test specimens,
- Hot tensile test Optional.
- Impact test is not performed for products with a thickness of less than 6 mm.
- A minimum impact energy value of 40 J may be requested, subject to agreement.
16MO3 (6345) Chemical analysis of quality boiler sheets
Alloy Steel Suitable for Use Under High Temperature and Pressure
Standard : EN 10028-2:2017
Chemical Composition (%)
|
|
Standard Equivalent
|
ERDEMİR
Quality No
|
C
|
Mn
|
P max.
|
S max.
|
Si
max.
|
N max.
|
Cr max.
|
Cu max.
|
Mo
|
Ni
max.
|
Standard
|
Quality
|
EN 10028-2
|
16Mo3
|
6345(1)
|
0.12-0.20
|
0.40-0.90
|
0.025
|
0.010
|
0.35
|
0.012
|
0.30
|
0.30
|
0.25-0.35
|
0.30
|
Descriptions
1) Products of this quality are produced in full stasis. Therefore, Al/N has a minimum ratio of 2:1
Mechanical Properties
|
|
Standard Equivalent
|
ERDEMİR
Quality No
|
Re N/mm2 (kg/mm2)
|
Rm(1) N/mm2 (kg/mm2)
|
A5 (%) min.
|
Coup(3)(4)
(Transverse)
|
Rp0.2(1)(2)
N/mm2 (kg/mm2)
Heat= 300°C
|
Sıc.
°C
|
KVc min.
J
|
d<16 min.
|
16<d<40 min.
|
40<d<60 min.
|
d<16 min.
|
16<d<40
min.
|
40<d<60 min.
|
Standard
|
Quality
|
EN 10028-2
|
16Mo3
|
6345
|
275
( 28.1 )
|
270 ( 27.6 )
|
260 ( 26.5 )
|
440 – 590
( 44.9 – 60.2 )
|
22
|
20
|
31
|
194 ( 19.8 )
|
190
( 19.4 )
|
183 ( 18.7 )
|
Descriptions
1-The tensile test values are applied to the ‘transverse’ test specimens.
2-Hot tensile test is done optionally.
3- Impact test is not performed for products with a thickness of less than 6 mm.
4-Depending on the agreement, a minimum impact energy value of 40 J may be requested.
Chemical Composition (%)
|
|
Standard Equivalent
|
ERDEMİR
Quality No
|
C
|
Mn
|
P max.
|
S max.
|
Si
max.
|
N max.
|
Cr max.
|
Cu max.
|
Mo
|
Ni
max.
|
Standard
|
Quality
|
EN 10028-2
|
16Mo3
|
6345(1)
|
0.12-0.20
|
0.40-0.90
|
0.025
|
0.010
|
0.35
|
0.012
|
0.30
|
0.30
|
0.25-0.35
|
0.30
|
|
Descriptions
1) Products of this quality are produced in full stasis. Therefore, the Al/N ratio is at least 2:1.
Mechanical Properties
|
|
Standard Equivalent
|
ERDEMİR
Quality No
|
Re N/mm2 (kg/mm2)
|
Rm(1) N/mm2 (kg/mm2)
|
A5 (%) min.
|
Coup(3)(4)
(Transverse)
|
Rp0.2(1)(2)
N/mm2 (kg/mm2)
Heat= 300°C
|
Sıc.
°C
|
KVc min.
J
|
d<16 min.
|
16<d<40 min.
|
40<d<60 min.
|
d<16 min.
|
16<d<40
min.
|
40<d<60 min.
|
Standard
|
Quality
|
EN 10028-2
|
16Mo3
|
6345
|
275
( 28.1 )
|
270 ( 27.6 )
|
260 ( 26.5 )
|
440 – 590
( 44.9 – 60.2 )
|
22
|
20
|
31
|
194 ( 19.8 )
|
190
( 19.4 )
|
183 ( 18.7 )
|
Descriptions
- The tensile test values are applied to the ‘transverse’ test specimens.
- Hot tensile test Optional.
- Impact test is not performed for products with a thickness of less than 6 mm.
- A minimum impact energy value of 40 J may be requested, subject to agreement.
ERDEMIR quality equivalent of P355GH quality steels is 6352 Quality. Erdemir 6352 quality boiler sheets have a very high resistance to pressure. In addition, there are steels used in the production of pressure resistant pipes produced by Erdemir.